The major alloy groups covered include aluminium, copper, nickel, titanium, and other nonferrous alloys. Major sections are devoted to carbon, alloy, stainless and pressure vessel steels, as well as to superalloys. The effect of variables, such as grain size, cooling rate, stress intensity, and temperature, are presented, along with numerous environments.